Product details
Titanium Anode for Copper Foil
The pretreatment of electrolyzing copper foil---Titanium Anode 1.Electrolyte :H2SO4(30%)+CuSO4
2.Current Density:3000A/M
3.Working Temperature:60℃
4.Service Life:≥2 Years(40 million hours)
5.Ph Value:Highly Acidic
6.Main Compositions:IrO2+X |